摘要 |
<p>A polymer composition includes a block copolymer, at least one oligomeric solvent, and at least one solid additive. The block copolymer is mixed with the solvent and the solid additive at a temperature above 150 °C to form the polymer composition. The solid additive blooms to the surface of the polymer composition during the useable life of polymer composition, thereby decreasing the shelf-life and usable life of parts, such as golf club grips, created therefrom.</p> |