摘要 |
The present disclosure relates to a method of consolidating a calcine comprising radioactive material, the method comprising mixing 60-80% (by weight) of a radionuclide containing calcine with at least one non-radioactive additive, such as an oxide, and hot isostatic pressing the mixture to form a stable monolith of glass/ceramic. In one embodiment, the ratio of radionuclide containing calcine to additives is about 80:20 by weight, wherein the non-radioactive additive comprises oxides such as BaO, CaO, Al2O3, TiO2, SiO2 and others, that combine with the waste elements and compounds to form a ceramic mineral or glass/ceramic material, after hot isostatic pressing. Non-limiting examples of mineral phases that may be formed are: hollandite (BaAl2Ti6O16), zirconolite (CaZrThO7), and perovskite (CaTiO3). |