摘要 <P>PROBLEM TO BE SOLVED: To provide a composite material for brazing having a low melting temperature and a method for manufacturing the same. Ž<P>SOLUTION: The composite material for brazing includes: a laminated filler metal layer 6 that contains a titanium component layer 4 having titanium or a titanium alloy as filler metal and a nickel component layer 5 having nickel or a nickel alloy as filler metal; a base material layer 7 that is joined to the laminated filler metal layer 6 and composed of a base material; and a melting temperature lowering material layer 8 that is interposed between the base material layer 7 and the laminated filler metal layer 6 and that is composed of a melting temperature lowering material. Ž<P>COPYRIGHT: (C)2011,JPO&INPIT Ž