Improving blackened silver alloy mass for making a jewelry, comprises suspending silver alloy yarn in a container, and heating at a specified temperature
摘要
<p>Improving blackened silver alloy mass comprises suspending silver alloy yarn in a container, and then heating at a temperature of 400-700[deg] C so that the percentage of sulfur in the silver alloy is higher than 13%.</p>