摘要 |
<P>PROBLEM TO BE SOLVED: To provide means for reducing a lamination deviation in a manufacturing process of a battery. <P>SOLUTION: The electrode, having a non-conductive porous body as a base material, is formed with a positive electrode active material, being held in a hole of a surface layer part of one side of the porous body and with a negative electrode active material, being held in a hole of a surface layer part of the other side. <P>COPYRIGHT: (C)2013,JPO&INPIT |