摘要 |
<p>There are provided, according to the present invention, a resin composition for hollow blow-molded article which is obtained in a high productivity on an industrial scale with excellent moldability and drawdown resistance, and the production method thereof, by melting and mixing a polyarylene sulfide resin including a terminal carboxyl group within the resin in an amount of 25 to 45 (µmol/g), and having a non-Newtonian index of 0.90 to 1.15 and also a melt viscosity as measured at 300°C within the range of 1,000 poise to 3,000 poise and an epoxy group-containing polyolefin so that the proportion of the epoxy group-containing polyolefin is 5 to 30 parts by mass with respect to 100 parts by mass of the polyarylene sulfide resin; and a hollow blow-molded article with excellent mechanical strength, such as the heat resistance and impact resistance, and surface appearance, and the production method thereof.</p> |