摘要 |
PURPOSE: A manufacturing method of red clay nano latex foam and red clay nano latex foam thereof are provided to prevent red clay nano particle from staining to be distributed to the latex foam. CONSTITUTION: A manufacturing method of red clay nano latex foam comprises: a step of mixing the red clay with water or mixture of liquid by processing the red clay to a particle size of 40-50nm(S100), a step of liquefying after absorbing the red clay nano to the surface of the curing agent or a catalyst by mixing the red clay nano with the curing agent(S200), and a step of impregnating by stirring the latex undiluted solution mixing additive including vulcanizing and curing agent, surfactant, antioxidant, anti-aging agent, and filler with red clay nano additive(S300), a step of molding mixed red clay nano latex mixture by a latex mold(S400), and a step of producing red clay nano latex finished product of far-infrared radiation by drying the red clay nano latex(S500). [Reference numerals] (S100) First liquid mixing step, Red clay nano + Water(distilled water); (S200) Second liquid mixing step, The mixture of the first liquid mixing step + Curing agent, catalyst; (S300) Stirring and impregnating step, The mixture of the second liquid mixing step + Vulcanizing agent, surfactant, additive; (S400) Foaming step; (S500) Finished product producing step, Far-infrared radiation red clay nano latex foam;
|