发明名称 Lighter than air balloon made from a biaxially oriented polyester film
摘要 A long life balloon formed from a lamination. The lamination includes a polyester film with a total thickness of 4 μm to 12 μm. The polyester film includes a biaxially oriented polyester core layer and at least one amorphous copolyester skin layer. The lamination also includes a sealant layer and a gas barrier layer on an opposite side of the polyester film from the sealant layer. The oxygen transmission rate of the balloon is less than 0.1 cc/100 sqin/day, a bonding strength of the gas barrier layer to the surface of the polyester film is more than 300 g/in at dry conditions, a sealing strength of the balloon is more than 3.5 kg/in, and a floating time of the balloon is more than 20 days.
申请公布号 US8399080(B2) 申请公布日期 2013.03.19
申请号 US20080202655 申请日期 2008.09.02
申请人 CHICARELLA GIANFRANCO;YOKOTA NAO;PAOLILLI TRACY A.;FITCH JOHN J.;SARNSTROM TODD R.;BORCHARDT DEAN;ANSOLABEHERE PAUL A.;SARGEANT STEVEN;TORAY PLASTICS (AMERICA), INC.;ANAGRAM INTERNATIONAL, INC. 发明人 CHICARELLA GIANFRANCO;YOKOTA NAO;PAOLILLI TRACY A.;FITCH JOHN J.;SARNSTROM TODD R.;BORCHARDT DEAN;ANSOLABEHERE PAUL A.;SARGEANT STEVEN
分类号 B32B1/00;B32B1/08 主分类号 B32B1/00
代理机构 代理人
主权项
地址