发明名称 Medium-low temperature sintered fine bone china and manufacturng method thereof
摘要 <p>The present invention relates to a medium-low temperature sintered fine bone china and a manufacturing method thereof. The chemical composition of the china is: SiO2 52 60%, Al2O3 28 37%, K2O 1 4%, Na2O 1 2%, CaO 3 8%, MgO 1 3%, and P2O5 1 3%; the materials used are: bone ash 3 8%, kaolin 32 45%, aluminum oxide 10 20%, and frit 35 50%, while the sintering temperature is between 1170 °C 1250 °C. A "high temperature bisque firing, low temperature glaze firing" or a "low temperature bisque firing, high temperature glaze firing" dual pass firing technique can be used; a high temperature single pass firing technique can also be used. The fine bone china of the present invention has the visual effect of traditional bone china, improved physical and chemical properties over bone china, and the advantages of a lower bone char usage and a lower firing temperature to enable lower production costs and energy consumption.</p>
申请公布号 GB2494568(A) 申请公布日期 2013.03.13
申请号 GB20120021966 申请日期 2011.07.05
申请人 JINGDEZHEN CERAMIC INSTITUTE 发明人 WEIHUI JIANG;LIFENG MIAO;ZHENHONG BAO;XUNYAN TAN;PENGPENG YU;JIANMIN LIU;QINGXIA ZHU
分类号 C04B35/185;C04B35/111;C04B35/622 主分类号 C04B35/185
代理机构 代理人
主权项
地址