摘要 |
FIELD: textile, paper.SUBSTANCE: method includes preparation of a paper base with weight of 55-90 g/mand specified parameters of absorbency with one-sided wetting and air permeability, application of a coating on it with weight of 6-12 g/m, consisting of a binder and a filler with their specified ratio, besides, the base is prepared with the value of absorbency in the range of 28-55 g/mby Cobband value of air impermeability in the range of 190-480 cm/min.EFFECT: possibility to reduce coating weight with preservation of printing quality when operating in wide ranges of filling density values and speed of images sealing.2 cl, 1 tbl |