发明名称 METHOD FOR PRODUCING POLYMER HAVING DESIRED CURIE TEMPERATURE
摘要 <P>PROBLEM TO BE SOLVED: To obtain a method which easily produces a polymer having a desired Curie temperature from a copolymer. <P>SOLUTION: The method for producing a polymer having a desired Curie temperature includes: a step (S01) of making a copolymer having a first Curie temperature into a solution or a melt; a step (S02) of making a copolymer having a second Curie temperature different from the first Curie temperature into a solution or a melt, wherein the monomer constituting the copolymer is the same monomer of the copolymer having the first Curie temperature; and steps (S03 and S04) of mixing the copolymer having the first Curie temperature with the copolymer having the second Curie temperature after dissolution or melting, and producing a polymer blend. The polymer produced by the method has a single Curie temperature determined by a mixing ratio of the copolymer having the first Curie temperature to the copolymer having the second Curie temperature. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013043903(A) 申请公布日期 2013.03.04
申请号 JP20110180742 申请日期 2011.08.22
申请人 KUREHA CORP 发明人 MORIYAMA NOBUHIRO;SUZUKI KEITARO
分类号 C08J3/20;C08F214/22;C08J5/18;C08L27/16;H01G4/18;H01L41/193;H01L41/45 主分类号 C08J3/20
代理机构 代理人
主权项
地址