摘要 |
A process for producing the alumina fiber aggregate which, when examined by the electron microscope method, gives a frequency distribution regarding number of fibers, wherein the number of fibers having a fiber length of 50-200 μm is 70% or more (including 100%), the number of fibers having a fiber length smaller than 50 μm is 30% or less (including 0), the number of fibers of 50-100 μm is 30-50%, the number of fibers longer than 100 μm but not longer than 200 μm is 30-50%, and the number of fibers longer than 200 μm is 20% or less (including 0). The process including the steps of grinding cottony alumina-based fibers comprising 70-100% by mass of Al2O3 and 0-30% by mass of SiO2 while applying a pressure of 0.1-20 MPa thereto and then classifying the ground fibers.
|