发明名称 TWO-WIRE WELDING CONTROL METHOD
摘要 <P>PROBLEM TO BE SOLVED: To improve welding efficiency by increasing the welding amount of a filler wire in a two-wire welding method for feeding the filler wire to a consumable electrode arc to weld the filler wire. <P>SOLUTION: The two-wire welding method includes: generating an arc between the consumable electrode and a base material to form a molten pool; and welding the filler wire while inserting the filler wire in the latter half part of the molten pool. In the method, the filler wire is weaved back and forth in a welding direction to change the displacement amount Lh of an inserted position of the filler wire in sinusoidal shape, and the feed speed Fw of the filler wire is changed in sinusoidal shape in proportion to the displacement amount Lh. Consequently, when the inserted position of the filler wire is in a forward direction from the center position of weaving, melting of the filler wire is accelerated, and the feed speed Fw of the filler wire is increased, and when the inserted position of the filler wire is in a backward direction, cooling and rising of the molten pool are suppressed, and the formation of a humping bead is suppressed. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013035020(A) 申请公布日期 2013.02.21
申请号 JP20110172840 申请日期 2011.08.08
申请人 DAIHEN CORP 发明人 SHIOZAKI HIDEO
分类号 B23K9/173;B23K9/022;B23K9/12 主分类号 B23K9/173
代理机构 代理人
主权项
地址