摘要 |
Provided is a ceramic electronic part wherein insulation of a magnetic material section can be secured, oxidation of Cu that is inner conductors can be inhibited, and excellent electrical characteristics can be achieved. A method of manufacturing a ceramic electronic part according to the present invention comprises a baking process for executing baking at a prescribed temperature rising rate (X) (°C/min) and at a prescribed oxygen partial pressure (Y) (Pa). The method of manufacturing a ceramic electronic part is characterized by executing baking in a condition prescribed by, when the temperature rising rate (X) is indicated as the x-axis and the oxygen partial pressure (Y) is indicated as the y-axis, an area in which (X, Y) is surrounded by A(50, 0.05), B(1000, 0.05), C(1000, 0.01), D(1500, 0.01), E(1500, 0.001), F(2000, 0.001), G(2000, 100), H(1500, 100), I(1500, 50), J(1000, 50), K(1000, 10), and L(50, 10). |