发明名称 Method for manufacturing reductive stone material using molten slag
摘要 A method for manufacturing a reductive stone material using a molten slag. The method comprises these steps: controlling the molten slag at a temperature between 1,400°C and 1,500°C, and cast molding at a controlled temperature; thermally insulating the molded molten slag at a temperature between 800°C and 1,000°C in a non-reductive atmosphere for one to five hours, and then cooling gradually to room temperature within two to five hours to acquire the reductive stone material. The method provides an energy conserving and high efficiency way of utilizing blast furnace slag. The reductive stone material produced is characterized by color stability, wear resistance, pressure resistance, non-flakiness, a low expansion coefficient, and a low contractability rate.
申请公布号 AU2011307776(A1) 申请公布日期 2013.02.07
申请号 AU20110307776 申请日期 2011.09.20
申请人 SHANDONG COKING GROUP CO., LTD. 发明人 WANG, QINGTAO;YU, XIANJIN;ZHAO, XIN;GONG, BENKUI;WEI, ZHENXIA;LI, YUEYUN;MING, JUN
分类号 C04B5/00;C04B5/06 主分类号 C04B5/00
代理机构 代理人
主权项
地址