发明名称 FIBER-CONTAINING CEMENT SLURRY
摘要 <P>PROBLEM TO BE SOLVED: To provide a fiber-containing cement slurry, wherein fiber is uniformly dispersed in a cement slurry without requiring complicated procedures. <P>SOLUTION: The fiber-containing cement slurry has physical properties in which: the viscosity of the cement slurry formed by mixing a cement, water and an additive, as measured with a rotating viscometer, falls within a range of 0.1 (solid line 80) to 3.8 (solid line 82) Pa_s; and the L-flow initial velocity of the cement slurry formed by mixing the cement, the water, the additive, and fiber falls within a range (shaded area S) of 13 (solid line 84) to 120 (solid line 86) cm/s. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013028474(A) 申请公布日期 2013.02.07
申请号 JP20110164512 申请日期 2011.07.27
申请人 TAKENAKA KOMUTEN CO LTD 发明人
分类号 C04B28/02;C04B16/06;C04B24/38;E02D3/12 主分类号 C04B28/02
代理机构 代理人
主权项
地址