摘要 <p>A method including forming a bilayer polymer film having an oriented polypropylene film and a metallocene-catalyzed polypropylene film wherein the metallocene-catalyzed polypropylene film has a seal initiation temperature of from 80° C. to 130° C. A laminate including a biaxially oriented polypropylene film, a metallocene-catalyzed polypropylene film, and a substrate, wherein the metallocene-catalyzed polypropylene film is disposed between the biaxially oriented polypropylene film and the substrate.</p>
申请公布号 JP2013503756(A) 申请公布日期 2013.02.04
申请号 JP20120527098 申请日期 2010.08.31
申请人 发明人
分类号 B32B27/32;B29C47/02;B29K23/00;B29L7/00;B29L9/00 主分类号 B32B27/32