发明名称 COATING MATERIAL OF SUPERCONDUCTING WIRE, SUPERCONDUCTING WIRE AND ELECTRICAL APPARATUS
摘要 <P>PROBLEM TO BE SOLVED: To provide a coating material for superconducting wire in which deterioration of the characteristics is minimized, and to provide a superconducting wire and an electrical apparatus. <P>SOLUTION: A coating material 10 for a superconducting wire has a tensile strength at break of 12.0 N/3 mm or higher, and a tensile break elongation of 12% or more at -196&deg;C. The coating material 10 preferably contains a base material 11 consisting of polyimide resin. Furthermore, the coating material 10 preferably includes a viscoelastic body layer 12 formed on one surface of the base material 11. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2013020725(A) 申请公布日期 2013.01.31
申请号 JP20110151054 申请日期 2011.07.07
申请人 NITTO DENKO CORP;NITTO SHINKO KK 发明人
分类号 H01B12/02;H01B17/60;H01F6/06 主分类号 H01B12/02