摘要 |
The use of thermoplastic molding materials comprising A) 10 to 98.8% by weight of a mixture formed from a1) 40 to 70% by weight of nylon-6,6 or nylon-4,6 or nylon-6 or mixtures thereof, a2) 30 to 60% by weight of a polyamide having a ratio of methylene to amide groups of 7 to 12, B) 1 to 50% by weight of a fibrous or particulate filler, C) 0.1 to 3% by weight of a lubricant, D) 0.05 to 3% by weight of a heat stabilizer, E) 0 to 40% by weight of further additives, where the sum of the percentages by weight A) to E) and a1) and a2) adds to 100%, for production of stress cracking- and corrosion-resistant moldings.
|