发明名称 METHOD FOR PRODUCING POROUS ALUMINUM MAGNESIUM TITANATE
摘要 The production method of the present invention is a method for producing porous aluminum magnesium titanate by forming a mixture containing Al source powder, Mg source powder, Ti source powder and Si source powder as well as a pore-forming agent to obtain a molded body; presintering the obtained molded body; and then sintering the presintered molded body, wherein the content of the pore-forming agent to a total of 100 parts by mass for the Al source powder, Mg source powder, Ti source powder and Si source powder is 5 to 30 parts by mass, the melting point of the Si source powder is 600 to 1300°C, when the elemental composition ratio of Al, Mg, Ti and Si in the mixture is represented by compositional formula (1): €ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒ€ƒAl 2(1-x) Mg x Ti (1+x) O 5 + aAl 2 O 3 + bSiO 2 €ƒ€ƒ€ƒ€ƒ€ƒ(1), x satisfies 0.05 ‰¤ x ‰¤ 0.15, a satisfies 0 ‰¤ a ‰¤ 0.1 and b satisfies 0.05 ‰¤ b ‰¤ 0.15, and the presintered molded body is sintered at 1300 to 1560°C.
申请公布号 EP2546212(A1) 申请公布日期 2013.01.16
申请号 EP20110753292 申请日期 2011.03.04
申请人 SUMITOMO CHEMICAL COMPANY, LIMITED 发明人 TOHMA, TETSURO;IWASAKI, KENTARO
分类号 C04B35/478;C04B35/634;C04B38/06;C04B111/00 主分类号 C04B35/478
代理机构 代理人
主权项
地址