摘要 |
<p>A process for producing a styrene acrylonitrile (SAN) resin having enhanced transparency or reduced haze includes exposing styrene monomers and acrylonitrile monomers to l,l-Di(tert-butylperoxy)cyclohexane, the l,l-Di(tert-butylperoxy)cyclohexane having a concentration between approximately 5 - 500 parts per million (ppm) relative to a total weight of the styrene monomers and acrylonitrile monomers; initiating polymerization reactions involving the styrene monomers and the acrylonitrile monomers exposed to the the l,l-Di(tert-butylperoxy)cyclohexane; continuing the polymerization reactions for a polymerization time period; stopping the polymerization reactions; and obtaining a SAN resin having a haze value significantly less than approximately 0.50 (e.g., less than or equal to approximately 0.45, 0.40, 0.35, 0.30, 0.25, 0.20, 0.15, or 0.10).</p> |
申请人 |
THAI ABS COMPANY LIMITED;PATTAMAMONGKOLCHAI, SOMCHAI;PHONGTHONG, RONNAPA;KWAMPIAN, SUTHEP |
发明人 |
PATTAMAMONGKOLCHAI, SOMCHAI;PHONGTHONG, RONNAPA;KWAMPIAN, SUTHEP |