摘要 |
The present application provides a high strength spring steel and a high strength spring that have superior corrosion fatigue strength. The spring steel comprises, in terms of percent by mass, 0.35-0.55% C, 1.60-3.00% Si, 0.20-1.50% Mn, 0.10-1.50% Cr and at least one element selected from 0.40-3.00% Ni, 0.05-0.50% Mo 0.05-0.50% V, the balance being at least substantially Fe and incidental elements and impurities. |