发明名称 METHOD FOR PRODUCING THERMOPLASTIC MOLDING COMPOUNDS ON THE BASIS OF STYRENE COPOLYMERS AND POLYAMIDE HAVING IMPROVED VISCOSITY
摘要 <p>The invention relates to a method for producing thermoplastic molding compounds, wherein the thermoplastic molding compounds contain a) 3 to 79 wt.% of one or more (meth)styrene-acrylonitrile copolymers, which comprise no units derived from maleic acid anhydride, as component A, b) 15 to 91 wt.% of one or more polyamides as component B, c) 5 to 50 wt.% of one or more rubbers as a component C, d) 1 to 25 wt.% of one or more compatibilizing agents as component D, e) 0 to 2 wt.% of one or more low-molecular-weight compounds, which contain a dicarboxylic acid anhydride group, as component E, f) 0 to 50 wt.% of one or more fiber- or particle-shaped fillers as component F, and g) 0 to 45 wt.% of additional additives as component G, wherein the wt.% in each case are relative to the total weight of the components A to G and together are 100 wt.%, by melt-mixing the components A to G, wherein it is essential to the invention that in a first method step, in the absence of component D, a melt containing components A, B and C is produced, and component D is admixed to said melt not until a subsequent second method step. The invention further relates to thermoplastic molding compounds that can be obtained according to said method, to the use of said thermoplastic molding compounds, and to molded bodies, fibers and film containing said thermoplastic molding compounds.</p>
申请公布号 EP2526152(A1) 申请公布日期 2012.11.28
申请号 EP20110700528 申请日期 2011.01.12
申请人 BASF SE 发明人 WEBER, MARTIN;BLINZLER, MARKO;GUENTHERBERG, NORBERT
分类号 C08L77/00;C08J3/00;C08K5/1539;C08K7/02;C08L25/12;C08L35/06;C08L51/04;C08L55/02;C08L77/02 主分类号 C08L77/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利