<P>PROBLEM TO BE SOLVED: To improve ease of peeling of an insulating composition in, for example, electric wire and cable terminal parts, by suppressing adhesion of a resin-mixed material with respect to a screw of an extrusion molding machine, or the like. <P>SOLUTION: A resin-mixed material is employed. The resin-mixed material is obtained by mixing 3-8 parts by weight of polyamide having a melting point of 190°C or below, plasticizer and thermal stabilizer with respect to at least 100 parts by weight of vinyl chloride resin. The resin-mixed material may be one which is obtained by mixing filler according to a target insulating composition. The resin-mixed material is used by coating it onto, for example, a peripheral surface of a wire-shaped conductor in electric wire and cable. <P>COPYRIGHT: (C)2013,JPO&INPIT |