发明名称 IRON-CHROMIUM ALLOY WITH IMPROVED COMPRESSIVE YIELD STRENGTH AND METHOD OF MAKING AND USE THEREOF
摘要 A chromium-iron alloy comprises in weight %, 1 to 3% C, 1 to 3% Si, up to 3% Ni, 25 to 35% Cr, 1.5 to 3% Mo, up to 2% W, 2.0 to 4.0% Nb, up to 3.0% V, up to 3.0% Ta, up to 1.2% B, up to 1% Mn and 43 to 64% Fe. In a preferred embodiment, the chromium-iron alloy comprises in weight %, 1.5 to 2.3% C, 1.6 to 2.3% Si, 0.2 to 2.2% Ni, 27 to 34% Cr, 1.7 to 2.5% Mo, 0.04 to 2% W, 2.2 to 3.6% Nb, up to 1% V, up to 3.0% Ta, up to 0.7% B, 0.1 to 0.6% Mn and 43 to 64% Fe. The chromium-iron alloy is useful for valve seat inserts for internal combustion engines such as diesel or natural gas engines.
申请公布号 EP2521800(A2) 申请公布日期 2012.11.14
申请号 EP20100842363 申请日期 2010.12.23
申请人 L.E. JONES COMPANY 发明人 QIAO, CONG YUE;TRUDEAU, TODD