发明名称 |
METHOD FOR PRODUCING POSITIVE ELECTRODE FOR NON-AQUEOUS ELECTROLYTE SECONDARY CELL AND METHOD FOR PRODUCING NON-AQUEOUS ELECTROLYTE SECONDARY CELL |
摘要 |
A method for producing a non-aqueous electrolyte secondary cell by preparing a positive electrode by applying a positive electrode mixture onto a positive electrode core material, the mixture containing a positive electrode active material mainly made of a lithium nickel composite oxide and a binding agent containing polyvinylidene fluoride; measuring the amount of carbon dioxide gas generated when a layer of the positive electrode mixture is removed out of the positive electrode and the layer is heated to 200° C. or higher and 400° C. or lower in an inactive gas atmosphere; selecting a positive electrode satisfying the following formulas: y<(0.27x−51)/1000000(200≦̸x<400)  formula 1 y<57/1000000(400≦̸x≦̸1500)  formula 2 where x is a heating temperature (° C.) and y is the amount of carbon dioxide gas (mole/g) per 1 g of the lithium nickel composite oxide measured; and preparing the non-aqueous electrolyte secondary cell by using the positive electrode selected. |
申请公布号 |
US2012280172(A1) |
申请公布日期 |
2012.11.08 |
申请号 |
US201213469747 |
申请日期 |
2012.05.11 |
申请人 |
TAKEDA KATSUTOSHI;KATO YOSHIO;TODE SHINGO;MAEKAWA MASANORI;MATSUTA SHIGEKI;SANYO ELECTRIC CO., LTD. |
发明人 |
TAKEDA KATSUTOSHI;KATO YOSHIO;TODE SHINGO;MAEKAWA MASANORI;MATSUTA SHIGEKI |
分类号 |
H01M4/525;H01M4/52;H01M10/36 |
主分类号 |
H01M4/525 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|