发明名称 HEAT-TREATMENT OF AN ALLOY FOR A BEARING COMPONENT
摘要 <p>A method for preparing a titanium alloy for a bearing component comprising: (i) providing an alloy composition comprising: from 5 to 7 wt% Al, from 3.5 to 6 wt% V, from 0.5 to 6 wt% Mo, from 0.2 to 4.5 wt% Fe, from 0.05 to 2.5 wt% Cr, optionally one or more of the following elements up to 2.5 wt% Zr, up to 2.5 wt% Sn, up to 0.5 wt% C, and the balance comprising Ti together with unavoidable impurities; (ii) heating the alloy to a temperature T below the (a+ß/ß)-transition temperature Tß and then quenching; and (iii) ageing the alloy at a temperature of from 400 to 600°C.</p>
申请公布号 WO2012146653(A2) 申请公布日期 2012.11.01
申请号 WO2012EP57642 申请日期 2012.04.26
申请人 AKTIEBOLAGET SKF;DE VRIES, ALEXANDER;SANZ, ALEJANDRO 发明人 DE VRIES, ALEXANDER;SANZ, ALEJANDRO
分类号 主分类号
代理机构 代理人
主权项
地址