发明名称 GLASS-REINFORCED RESIN COMPOSITION
摘要 <P>PROBLEM TO BE SOLVED: To provide a glass-reinforced resin composition excellent in thermal stability and mechanical strength, and small in anisotropy of mold shrinkage factor thereby suppressing warpage. <P>SOLUTION: This glass-reinforced resin composition includes (B) 1-150 pts.wt. of glass flake (component B) with an averaged thickness of 0.2-0.7 &mu;m, and (C) 0.0001-1.0 pt.wt. of a surface-treatment deactivator (component C), based on (A) 100 pts.wt. of a thermoplastic resin (component A), wherein the amount of a surface-treating agent of the glass flake is 1.5-5 pts.wt. based on 100 pts.wt. of the glass flake. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2012207075(A) 申请公布日期 2012.10.25
申请号 JP20110072102 申请日期 2011.03.29
申请人 TEIJIN CHEM LTD 发明人 MURAI MAIKO;IKEMATSU RYUSUKE
分类号 C08L101/00;C08K5/49;C08K7/00;C08L69/00 主分类号 C08L101/00
代理机构 代理人
主权项
地址