摘要 |
A cured fluoroelastomer sensor bushing comprises A) fluoroelastomer having at least 53 wt. % fluorine, and B) 10 to 50 parts by weight, per hundred parts by weight fluoroelastomer, of carbon black a nitrogen adsorption specific surface area of 70-150 m2/g and a dibutyl phthalate absorption of 90-180 ml/100 g. |