摘要 A cooling method of steel plate able to raise a cooling uniformity in a steel plate conveyance direction comprising, at a front stage part of a cooling apparatus, not spraying while a front end region of steel plate is passing, spraying by successively increasing the cooling water rate from 80 to 95 vol % (Qfront) of a standard water density when the front part region passes so that the amount of cooling water becomes the standard water density when a boundary part of the front part region and a center part region arrives, and continuing spraying by the standard water density while the center part region is passing, then, at a rear stage part of the cooling apparatus, spraying by making the amount of cooling water 80 to 95 vol % of the standard water density while the front end region of the steel plate is passing, successively increasing the amount of cooling water rate from 80 to 95 vol % of the standard water density when the front part region passes so that the amount of cooling water becomes the standard water density when the boundary part of the front part region and the center part region arrives, and continuing spraying by the standard water density while the center part region is passing.
申请公布号 US8282747(B2) 申请公布日期 2012.10.09
申请号 US20070223367 申请日期 2007.07.31
申请人 ODA TOMOYA;NIPPON STEEL CORPORATION 发明人 ODA TOMOYA
分类号 C21D6/00 主分类号 C21D6/00
代理机构 代理人
主权项
地址