发明名称 CATALYST, AND METHOD FOR PRODUCING THE SAME
摘要 <P>PROBLEM TO BE SOLVED: To provide a catalyst that has an enlarged particle diameter of a composite oxide particle without input of an excessive amount of energy, and to provide a method for producing the same. <P>SOLUTION: The catalyst includes a metal fine particle composed of at least one selected from nickel, cobalt, iron and copper on a surface of the composite oxide particle composing a composite oxide sintered body containing at least one selected from nickel, cobalt, iron and copper, and at least one selected from aluminum, magnesium and chromium, wherein the composite oxide sintered body contains a vanadium component. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP2012187495(A) 申请公布日期 2012.10.04
申请号 JP20110052582 申请日期 2011.03.10
申请人 TOSHIBA CORP 发明人 FUKAZAWA TAKAYUKI;KOSHIZAKI KENJI;OSADA NORIKAZU
分类号 B01J23/847;B01J23/86;B01J31/08;B01J37/04;B01J37/16;C01B3/32;C01B3/40;C01B31/02 主分类号 B01J23/847
代理机构 代理人
主权项
地址