摘要 |
Disclosed is a multilayer blow-molded container having high gloss, excellent surface appearance and excellent impact resistance. The multilayer blow-molded container is characterized in that a resin to be used for the outermost layer comprises an olefin polymer composition (E) comprising a propylene resin (A), an ethylene·a-olefin copolymer (B) and a nucleating agent (D), the propylene resin (A) comprises a copolymer of propylene and an a-olefin (A-1) and has a crystal melting point of 140 to 155°C (A-2), the ethylene·a-olefin copolymer (B) comprises a copolymer of ethylene and at least one a-olefin having 4 to 20 carbon atoms (B-1) and has a crystal melting point of not lower than 85°C and lower than 110°C (B-2), and the olefin polymer composition (E) has an MFR value of 5 to 10 g/10 min (E-1). |