发明名称 STEAM TURBINE ROTOR
摘要 <P>PROBLEM TO BE SOLVED: To improve a durable temperature to 760-800&deg;C while maintaining hot workability. <P>SOLUTION: A Ni-based forging alloy contains: 0.001-0.1 wt.% of C; 12-23 wt.% of Cr; 3.5-5.0 wt.% of Al; and inevitable impurities, and the balance comprises Ni. The sum of W and Mo is 5-12 wt.%; the Mo is 5 wt.% or less; and the added amount of Ti, Ta and Nb is practically zero. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012177370(A) 申请公布日期 2012.09.13
申请号 JP20120095206 申请日期 2012.04.19
申请人 HITACHI LTD 发明人 KONNO SHINYA;DOI HIROYUKI;SATO JUN
分类号 F01D5/00;C22C19/05;F01D25/00 主分类号 F01D5/00