发明名称
摘要 <p>A method of shaping a region (26) on a glass ribbon (20), the glass ribbon including a softening point, and a thickness (24). The method includes, at a location where the glass ribbon has a viscosity less than or equal to 7x1014 poise: causing the region of the glass ribbon to be at a temperature at or above the softening point temperature; and applying tension (35, 37) to the glass ribbon, across the region, so as to form a necked-down section (27) in the region, wherein the necked-down section has a thickness (28) that is less than the thickness of the glass ribbon on each side of the region. Non-sharp portions (29) may be formed together with the necked-down section. The ribbon may then be broken along the necked-down section to separate portions from one another.</p>
申请公布号 JP2012519136(A) 申请公布日期 2012.08.23
申请号 JP20110552153 申请日期 2010.02.25
申请人 发明人
分类号 C03B17/06 主分类号 C03B17/06
代理机构 代理人
主权项
地址