A thermoplastic resin composition and a method of producing the thermoplastic resin composition are provided. The thermoplastic resin composition has an excellent balance of flexibility, heat resistance, and abrasion resistance, and has an excellent moldability. The method includes the steps of heating in which a heat-processed product is heated at a maximum heating temperature of 327° C. or higher, the heat-processed product being obtained by heat-processing a mixture containing the thermoplastic resin and the PTFE particles; and cooling in which the heat-processed product is cooled at a cooling speed of 10° C./min or slower to 293° C. from the maximum heating temperature after the step of heating. |