发明名称 POROUS MOLDING
摘要 <P>PROBLEM TO BE SOLVED: To provide a porous molding excellent in crack resistance when a temperature is changed repeatedly from a high temperature to a low temperature. <P>SOLUTION: The porous molding excellent in crack resistance contains silicoaluminophosphate (SAPO), for example, SAPO-34 and/or aluminophosphate (ALPO) having a positive coefficient of linear expansion, and ALPO, for example, AIPO-D having a negative coefficient of linear expansion. A weight ratio (X)/(Y) between the weight (X) of SAPO and/or ALPO having a positive coefficient of linear expansion and the weight (Y) of ALPO having a negative coefficient of linear expansion is in the range of 0.125-9. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012136407(A) 申请公布日期 2012.07.19
申请号 JP20100291282 申请日期 2010.12.27
申请人 JGC CATALYSTS & CHEMICALS LTD 发明人 MITSUI TOMOHIRO;MORISHITA YUKA;MIZUNO TAKAYOSHI;KOYANAGI TSUGUO
分类号 C01B39/54;B01D53/94;B01J29/85;F01N3/08 主分类号 C01B39/54
代理机构 代理人
主权项
地址