发明名称 RUBBER COMPOSITION
摘要 <P>PROBLEM TO BE SOLVED: To provide a rubber composition which can suppress large decrease of tensile elongation, and can achieve high elasticity while securing processability. <P>SOLUTION: The rubber composition includes: 0.5-40 pts.mass of a thermoplastic polyester resin having at most 130&deg;C of a glass transition point and at least 20.0 of an SP value based on 100 pts.mass of a low polarity diene-based rubber (natural rubber, polybutadiene rubber, styrene butadiene rubber or the like) having less than 17.2 of an SP value (MPa)<SP POS="POST">1/2</SP>; and 2-30 mass% of a high polarity diene based rubber (nitrile rubber, epoxidation natural rubber or the like) having at least 17.2 and less than 20.0 of an SP value and at least 50,000 of a number average molecular weight based on the thermoplastic polyester resin. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012136586(A) 申请公布日期 2012.07.19
申请号 JP20100288576 申请日期 2010.12.24
申请人 TOYO TIRE & RUBBER CO LTD;TOYOBO CO LTD 发明人 KOJIMA MASAAKI;HISHIKAWA YASUHIRO;KITSUMOTO HIROTOSHI;UENO HITOSHI
分类号 C08L9/00;C08K3/04;C08L67/00 主分类号 C08L9/00
代理机构 代理人
主权项
地址