发明名称 |
FUSER MEMBER AND METHOD OF MANUFACTURING THE SAME |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide a fuser roller having a lifespan equal to or longer than a lifespan of an image forming apparatus. <P>SOLUTION: The method includes anodizing an outer surface of an aluminum substrate 300 to create an aluminum oxide surface layer 315 containing pores. The pores are impregnated with a fluorine-containing sealant selected from the group consisting of nickel fluoride and polytetrafluoroethylene. <P>COPYRIGHT: (C)2012,JPO&INPIT |
申请公布号 |
JP2012128416(A) |
申请公布日期 |
2012.07.05 |
申请号 |
JP20110268393 |
申请日期 |
2011.12.07 |
申请人 |
XEROX CORP |
发明人 |
GEORGE C CARDOZO;PINYIN LIN;ANTHONY S CONDELLO;JASON M LEFEVRE;SEYFRIED RICHARD W;GRACE T BREWINGTON;CHRISTOPHER LIN;DILL R MASHUTEA;JAMES R BEACHNER;DANIEL M BRAY |
分类号 |
G03G15/20;C08K3/16;C08L27/18 |
主分类号 |
G03G15/20 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|