摘要 The present invention relates to a method for producing a crumb rubber modified asphalt comprising the steps of: a) heating a pre-selected quantity of asphalt to a temperature of between about 325° F. to 550° F.; b) adding crumb rubber and a mineral acid to the heated asphalt with stirring; and c) blowing air through the asphalt, crumb rubber and mineral acid mixture.