<P>PROBLEM TO BE SOLVED: To provide a method of manufacturing a container using an environmentally friendly composition reducing manufacturing costs, being excellent in durability, water resistance and chemical resistance, and providing a variety of hues and forms. <P>SOLUTION: This method includes steps of: preparing the environmentally friendly composition made by mixing 10-90 pts.wt. of at least one of porous and harmless loess, kaolin, clay and powder blue clay, 15-25 pts.wt. of easily biodegradable resin coating agent, 0.1-25 pts.wt. of inorganic pigment, and 1-60 pts.wt. of water; and inputting the environmentally friendly composition into a molding machine at temperature of 50-200°C and at internal pressure of 1-10 kg/cm<SP POS="POST">2</SP>to mold at interval of 10 seconds to 5 minutes. <P>COPYRIGHT: (C)2012,JPO&INPIT |