摘要 |
The invention concerns a method for the preparation of finely divided calcium hydroxide, where burnt lime or calcium oxide is comminuted in an impact disintegrator (10), into which in addition to the calcium oxide part of the required amount of water led to wet the particles obtained, to bind the dust and to initiate the reaction, and the material comminuted and wetted in the impact disintegrator is led into a screw conveyor (20) being in connection with the impact disintegrator. The invention is characterized in that - the reaction is essentially completed in the screw conveyor (20) by feeding into the same the remainder of the amount of water needed for the reaction, and that - the temperature of the material in the last part of the screw conveyor is kept at a target temperature, which is essentially the vaporization temperature for water at the prevailing pressure, and the material is kept at the target temperature for a certain period of time, about 5...15 s, preferably about 10 s. |