摘要 |
<P>PROBLEM TO BE SOLVED: To provide a release film for molding a ceramic green sheet which can prevent heaving of a lug in a ceramic green sheet to be molded and shows successful coating properties for ceramic slurry and to provide a method for producing the release film. <P>SOLUTION: The release film 1 for molding the ceramic green sheet includes a base material 11 and a release agent layer 12 formed at least on one side surface of the base material 11. In the release film 1, when ethanol 12.0 mg is dropped onto a surface of the release agent layer 12 having 45° inclination to a level surface, time necessary for 100 mm movement of an ethanol droplet is 3.4 seconds or more. <P>COPYRIGHT: (C)2012,JPO&INPIT |