摘要 |
<P>PROBLEM TO BE SOLVED: To provide a laminate where a surface protection adhesive film is resistant to peel-off from an optical film, developability is superior, and an adhesive deposit is suppressed after peel-off from the optical film. <P>SOLUTION: An adhesive layer 6 has a copolymer including a polymer block A or B within a range where a weight ratio (A:B) is 5:95-25:75, or a hydrogen additive of the copolymer. Moreover, the laminate includes the surface protection adhesive film having an adhesive applying agent having 20 or more parts per weight relative to the total weight of 100 parts per weight of the copolymer and a softener, and the optical film 2 to which antistatic treatment is applied. <P>COPYRIGHT: (C)2012,JPO&INPIT |