摘要 |
PURPOSE: An algae growth inhibiting method using ammonium organo-nanoclay and a manufacturing method of an ammonium organo-nanoclay are provided to minimize ecosystem influence and prevent residual toxicity. CONSTITUTION: A manufacturing method of ammonium organic nanoclay comprises a step of mixing Amino-silane with metal positive ion precursor. The amino-silane is one selected from (3-(2-aminoethylamino)propyl)trimethoxysilane and 3-[2-(2-aminoethylamino)ethylamino]propyltrimethoxysilane. The mixing is processed at 5-30 deg. Celsius, and under 1 pressure. The metal positive ion precursor includes one metallic ion which is selected from Mg2+, Ca2+, Zn2+, Ni2+, Cu2+, Mn2+, Al3+, and Fe3+. The algal growth inhibiting method uses ammonium organic nanoclay. A concentration of the ammonium organic nanoclay is 0.10-100mg/L. The amino-silane is represented by chemical formula 1. |