发明名称
摘要 PROBLEM TO BE SOLVED: To provide a (K1-xNx)NbO3 piezoelectric ceramic composition having a high mechanical quality coefficient Qm, and low initial value of the dielectric loss tan&delta; and to provide a (K1-xNax)NbO3 piezoelectric ceramic composition having excellent long-term stability of the dielectric loss tan&delta;. SOLUTION: The piezoelectric ceramic composition has the composition expressed by general formula (K1-xNax)1-yAgy}NbO3-z[Ma&alpha;+][O2-]&alpha;/2, wherein x, y, z satisfy 0<=x<1, 0<=y<=0.1, 0<=z<=0.05 and y+z>0. In the formula, M is at least one kind of metal element selected from Mn, Mg, In, Si, Ga and Sb and &alpha; is the average valance of the metal element M.
申请公布号 JP4929522(B2) 申请公布日期 2012.05.09
申请号 JP20000254909 申请日期 2000.08.25
申请人 发明人
分类号 C04B35/00;G01L1/16;C04B35/495;H01L41/187 主分类号 C04B35/00
代理机构 代理人
主权项
地址