发明名称 |
METHOD FOR PREPARING A METAL OXIDE CATALYST FOR DEODORIZATION |
摘要 |
PURPOSE: A method for manufacturing metal oxide catalyst for deodorization is provided to save costs required for manufacturing catalyst by naturally drying the catalyst without a drying furnace. CONSTITUTION: A method for manufacturing metal oxide catalyst for deodorization includes the following: 1-50 weight% of manganese oxide of nano particles based on manganese nitrate solution is diluted into a colloidal form. The colloidal solution of the manganese nitrate containing manganese oxide at a temperature of 30 to 70 degrees Celsius is prepared. 10-20% of potassium permanganate is molten in distilled water of 65 to 75 degrees Celsius to obtain an aqueous solution. 1-30% of titanium dioxide of nano particles is diluted in the distilled water such that the titanium dioxide becomes a colloidal form. The titanium dioxide of colloidal form is mixed with the potassium permanganate and is heated in a double boiler. The mixture solution at a temperature of 50 to 70 degrees Celsius is prepared. 1-50% of auxiliary catalyst is diluted in distilled water of 50 to 80 degrees Celsius such that the auxiliary catalyst becomes a colloidal form, and an auxiliary catalyst impregnated support is dried. |
申请公布号 |
KR101132187(B1) |
申请公布日期 |
2012.04.06 |
申请号 |
KR20100113714 |
申请日期 |
2010.11.16 |
申请人 |
LEE, SUN KWEON |
发明人 |
LEE, SUN KWEON;KIM, JOONG KWON;KIM, NAM JUNG |
分类号 |
B01J23/889;A61L9/01;B01J23/34;B01J37/02 |
主分类号 |
B01J23/889 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|