摘要 |
The present invention provides a method of manufacturing an active material which can form an electrochemical device excellent in discharge capacity. The method of manufacturing an active material in accordance with the present invention comprises a hydrothermal synthesis step of heating a mixture including a lithium compound, a metal compound containing one species selected from the group consisting of Fe, Mn, Co, Ni, and V, a phosphorus compound, and water within a reactor while keeping an internal pressure of the reactor at 0.3 MPa or lower by ventilating the inside of the reactor to the outside, and closing the reactor at a time when the temperature of the mixture reaches 100 to 150° C.; and a firing step of firing the mixture after the hydrothermal synthesis step.
|