发明名称 Method of production of steel superior in machinability
摘要 The present invention provides steel superior in machinability comprised of, by wt %, C: 0.005 to 0.2%, Si: 0.001 to 0.5%, Mn: 0.2 to 3.0%, P: 0.001 to 0.2%, S: 0.03 to 1.0%, T.N: 0.002 to 0.02%, T.O: 0.0005 to 0.035%, and the balance of Fe and unavoidable impurities, said steel satisfying one or both of Mn/S in the steel being 1.2 to 2.8 or an area ratio of pearlite over a grain size of 1 μm in a microstructure of the steel being not more than 5%.
申请公布号 US8137484(B2) 申请公布日期 2012.03.20
申请号 US20080288542 申请日期 2008.10.20
申请人 HASHIMURA MASAYUKI;MIZUNO ATSUSHI;NAITO KENICHIRO;HAGIWARA HIROSHI;ISOBE KOHICHI;HIRATA HIROSHI;NIPPON STEEL CORPORATION 发明人 HASHIMURA MASAYUKI;MIZUNO ATSUSHI;NAITO KENICHIRO;HAGIWARA HIROSHI;ISOBE KOHICHI;HIRATA HIROSHI
分类号 C21D7/13;C21D8/00;C22C38/00;C22C38/04;C22C38/60 主分类号 C21D7/13