摘要 |
<P>PROBLEM TO BE SOLVED: To provide a vulcanized rubber laminated body having a sufficient adhesive force even if exposed to severe conditions (for example, immersed in fuel oil) in the vulcanized rubber laminated body where an unvulcanized epichlorohydrin based rubber composition layer and an unvulcanized fluororubber composition layer are heated, vulcanized and adhered. <P>SOLUTION: In the laminated body where (A) the unvulcanized epichlorohydrin based rubber composition layer and (B) the unvulcanized fluororubber composition layer are heated, vulcanized and adhered, in the laminated body for the fuel oil, (A) the unvulcanized epichlorohydrin based rubber composition layer contains the following (a)-(c). (a) The epichlorohydrin based rubber, (b) a vulcanizing agent, and (c) a specified polyether compound having a number average molecular weight of 1,000 or larger. <P>COPYRIGHT: (C)2012,JPO&INPIT |