发明名称 POLYMER MIXTURE CONSISTING OF IMPACT-MODIFIED POLY(METH)ACRYLATE AND FLUOROPOLYMER
摘要 <P>PROBLEM TO BE SOLVED: To provide a molding body having a material thickness of at least 150 &mu;m, which does not exhibit embrittlement at all or exhibits very low embrittlement if any, after prolonged thermal load. <P>SOLUTION: The molding body contains a polymer mixture composed of: impact-modified poly(meth)acrylate-plastic, consisting of a poly(meth)acrylate-matrix and elastomer particles distributed therein; and a fluoropolymer. The fraction of the fluoropolymer in the mixture is 30 to 95 mass%, and the mixture is composed of the plastic with a material thickness of at least 150 &mu;m present in an outer layer with a continuous material thickness of at least 10 &mu;m. Then, the impact-modified poly(meth)acrylate-plastic consists of: 20 to 70 mass% poly(meth)acrylate-matrix; and 80 to 30 mass% elastomer particles. <P>COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP2012052139(A) 申请公布日期 2012.03.15
申请号 JP20110259371 申请日期 2011.11.28
申请人 EVONIK ROEHM GMBH 发明人 ARNDT THOMAS;NUMRICH UWE;DEUSCH NORBERT;KROHMER CHRISTOPH
分类号 C08J5/00;B32B27/08;B32B27/28;B32B27/30;C08L27/12;C08L27/16;C08L33/10;C08L33/12;C08L51/00;C08L51/04;C08L51/06;C08L55/02 主分类号 C08J5/00
代理机构 代理人
主权项
地址